Conductor:
Annealed Copper Wire,(Bare Single,Tinned Single, Tinned Strand,or Top-Tinned Strand)
Insulation:
SR-PVC (Semi-Rigid Polyvinyl Chloride) or XLPVC (Cross-Linked Polyvinyl Chloride)
Structure:
Conductor |
Insulation |
Conductor
Resistance(20℃) |
AWG |
Construction |
Diameter |
Min
Thickness |
Nominal
Thickness |
Diameter |
32 |
7 / 0.08TA |
approx.0.24 mm |
0.14 mm |
0.18 mm |
0.60 ± 0.10 mm |
597.11W / Km |
30 |
7 / 0.10TA |
approx.0.30 mm |
0.16 mm |
0.20 mm |
0.70 ± 0.10 mm |
354.33W / Km |
28 |
7 / 0.13TA |
approx.0.39 mm |
0.205 mm |
0.80 ± 0.10 mm |
223.75W / Km |
26 |
7 / 0.16TA |
approx.0.48 mm |
0.21 mm |
0.90 ± 0.10 mm |
139.76W / Km |
28 |
1 / 0.32TA |
approx.0.32 mm |
0.19 mm |
0.24 mm |
0.80 ± 0.10 mm |
232.28W / Km |
32 |
7 / 0.08ATC |
approx.0.23 mm |
0.12 mm |
0.155 mm |
0.55 ± 0.10 mm |
578W / Km |
30 |
7 / 0.10ATC |
approx.0.29 mm |
0.14 mm |
0.175 mm |
0.65 ± 0.10 mm |
359.50W / Km |
28 |
7 / 0.13ATC |
approx.0.38 mm |
0.14 mm |
0.18 mm |
0.75 ± 0.10 mm |
229.40W / Km |
Note:TA:Tinned Copper , ATC:Top – Tinned Strand
Characteristics:
Items |
Specification |
Rating |
UL:80℃ 30V |
Dielectric Strength |
AC 1500V / min. |
Insulation Resistance |
Min. 5MW - Km (20℃) at DC 500V |
Flame Test |
UL: VW-1 |
Elongation of Insulation |
Min.100 ﹪ |
Tensile Strength of Insulation |
Min.1.05Kg / mm2 |
Residual of Elongation after Aging |
Min. 65 ﹪of original (113℃,168H) |
Residual of Tensile Strength after Aging |
Min. 70 ﹪of original (113℃,168H) |
|